MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ovako 100CrMo7-3 825B Steel, Q/T (martensite)
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: General Information: Ovako 825 is a through hardening bearing steel that is mainly used for medium sized bearing rings, but it can also be used for machine components that require high tensile strength, hardness and toughness.
  • Through hardenability corresponding to a ring with approximately 30mm wall thickness (˜Ø50mm bar), quenched in oil
  • Suitable for martensitic or banitic hardening
  • Good machinability in soft annealed condition
  • Good dimensional stabilityBQ-Steel:
    825B – Standard825T - With a controlled low sulphur content to minimize the number of sulphide inclusions. Reduced carbon content and tighter chemical composition ranges

    IQ-Steel:825Q - Isotropic properties (IQ) and better fatigue strength due to higher cleanliness levels, and a finer size and distribution of non-metallic inclusions

    BQ-Steel:BQ-steel® is a bearing quality clean steel optimized for fatigue strength and is also ideal for new design solutions outside the bearing industry.

    IQ-Steel:IQ-Steel® is an isotropic quality ultra clean steel optimized for high fatigue strength under multi axial loading.

    Information provided by Ovako

  • Key Words: A485 (B6)
    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 7.80 g/cc0.282 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell C 61
    @Thickness <=30.0 mm
    61
    @Thickness <=1.18 in
    Tensile Strength 2300 MPa
    @Thickness <=30.0 mm
    334000 psi
    @Thickness <=1.18 in
    Tensile Strength, Yield >= 1700 MPa
    @Thickness <=30.0 mm
    >= 247000 psi
    @Thickness <=1.18 in
    Modulus of Elasticity 210 GPa30500 ksi
    Poissons Ratio 0.300.30
    Shear Modulus 80.0 GPa11600 ksi
     
    Electrical PropertiesMetricEnglishComments
    Electrical Resistivity 0.00000200 - 0.00000250 ohm-cm0.00000200 - 0.00000250 ohm-cm
     
    Thermal PropertiesMetricEnglishComments
    CTE, linear 12.0 µm/m-°C
    @Temperature 20.0 - 300 °C
    6.67 µin/in-°F
    @Temperature 68.0 - 572 °F
    Specific Heat Capacity 0.460 - 0.480 J/g-°C
    @Temperature 50.0 - 100 °C
    0.110 - 0.115 BTU/lb-°F
    @Temperature 122 - 212 °F
    Thermal Conductivity 40.0 - 45.0 W/m-K278 - 312 BTU-in/hr-ft²-°FAmbient temperature
    Transformation Temperature 183 °C361 °FMS
     750 °C1380 °FAC1
     750 °C1380 °FAC3
     
    Component Elements PropertiesMetricEnglishComments
    Carbon, C 0.93 - 1.05 %0.93 - 1.05 %
    Chromium, Cr 1.65 - 1.95 %1.65 - 1.95 %
    Iron, Fe 95.16 - 96.42 %95.16 - 96.42 %As Balance
    Manganese, Mn 0.60 - 0.80 %0.60 - 0.80 %
    Molybdenum, Mo 0.20 - 0.35 %0.20 - 0.35 %
    Nickel, Ni <= 0.25 %<= 0.25 %
    Phosphorus, P <= 0.025 %<= 0.025 %
    Silicon, Si 0.20 - 0.40 %0.20 - 0.40 %
    Sulfur, S 0.0050 - 0.015 %0.0050 - 0.015 %

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Ovako 100Cr6 803Q Steel, Q/T (martensite)
    CMT CFR-AMC Fully Reinforced Aluminum Matrix Composite
    MMCC Al/Al2O3 Continuous Fiber Aluminum Matrix Composite
    ATI Allvac® 6-2-4-6 Titanium Alloy, Heat Treatment: 885°C (1625°F) + Age
    ATI Allvac® 6-4 Titanium Alloy, Heat Treatment: 704°C (1300°F) Anneal

    NOVAKO050 / 234349

    Aluminum Castings

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.