MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Michelman® FiberMax® 105B Strength enhancing fiber treatment  (discontinued **)
Categories: Fluid; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Description: Strength enhancing fiber treatment

Usage: FibreMax® 105B is a new alternative to paraffin wax for treating medium. It is a repulpable, machine ready, fiber treatment that increases the strength of paper and corrugated containers under humid conditions. FibreMax® 105B should not interfere with gluability.

Application data: FibreMax®105B can be applied by blade, rod or roll coater.

Food Contact Information when manufactured in the USA:
FDA:
175.105: Components of adhesives

Information provided by Michelman®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 - 1.06 g/cc1.04 - 1.06 g/cc
pH 9.0 - 10.59.0 - 10.5
Brookfield Viscosity 25 - 50 cP25 - 50 cPSpindle # 2, rpm 60
Viscosity Measurement 16 - 2016 - 20[sec], EZ cup, Cup # 2
 
Descriptive Properties
AppearanceOff-white, thin, opaque liquid
Solids TypeSynthetic

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Fibermax Bulk Mullite High-Temperature Fiber
Versalis SINKRAL G320 ABS

WMICHEL019 / 134936

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.