MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Crucible Steel Aquamet® 19 Stainless Steel
Categories: Metal; Ferrous Metal; Austenitic; Stainless Steel

Material Notes: AQUAMET 19 is a modified Type 304 stainless steel that is fully austenitic and non-magnetic. Strengthened by adding nitrogen to the melt, it has better corrosion resistance than Type 304 stainless. AQUAMET 19 has proven itself in demanding service on shrimpers, crabbers, scallopers, and other fishing boats as well as on pleasure craft. It may be considered as an economical alternative to AQUAMET 22.

Information provided by Crucible Specialty Metals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  655 MPa
@Thickness 76.2 - 305 mm
95000 psi
@Thickness 3.00 - 12.0 in
 896 MPa
@Thickness <=38.1 mm
130000 psi
@Thickness <=1.50 in
Tensile Strength, Yield  345 MPa
@Strain 0.2 %,
Thickness 76.2 - 305 mm
50000 psi
@Strain 0.2 %,
Thickness 3.00 - 12.0 in
Tension
 724 MPa
@Strain 0.2 %,
Thickness <=38.1 mm
105000 psi
@Strain 0.2 %,
Thickness <=1.50 in
Tension
Elongation at Break 35 %35 %in 2"; 3" to 12"
 20 %
@Thickness <=38.1 mm
20 %
@Thickness <=1.50 in
in 2"
Reduction of Area 55 %55 %
Shear Strength  228 MPa
@Strain 0.2 %,
Thickness 76.2 - 305 mm
33000 psi
@Strain 0.2 %,
Thickness 3.00 - 12.0 in
 483 MPa
@Strain 0.2 %,
Thickness <=38.1 mm
70000 psi
@Strain 0.2 %,
Thickness <=1.50 in
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.080 %<= 0.080 %
Chromium, Cr 18 - 20 %18 - 20 %
Iron, Fe >= 66.05 %>= 66.05 %As Remainder
Manganese, Mn <= 2.0 %<= 2.0 %
Nickel, Ni 8.0 - 10.5 %8.0 - 10.5 %
Nitrogen, N 0.20 - 0.30 %0.20 - 0.30 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si <= 1.0 %<= 1.0 %
Sulfur, S <= 0.030 %<= 0.030 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Crucible Steel Aquamet® 17 Martensitic Steel
Crucible Steel Aquamet® 22 Stainless Steel
Type 431 Martensitic Stainless Steel, Intermediate Temper Forgings, UNS S43100
Crucible Steel 431 Chromium Steel
Crucible Steel Aquamet® 18 Stainless Steel

NCRUC030 / 16023

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.