Uses: Chemical processing equipment, high-strength pump shafts, surgical implants, intermedullary nails, plates, screws, wires. Property values are for samples in the metallurgical condition: 1900°F 1 hr. + water quench. |
AMS 5764; ASTM A 182, A 184, A 193, A 194, A 240, A 249, A 269, A 312, A 336, F 1314. Formerly Nickelvac® XM-19 |