MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

MTM Plastics Dipolen® H Recycled HDPE Blend
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Dipolen® H is a granulated HDPE with other polyolefin blend for use in either extrusion or injection molding. It can be supplied unmodified or treated with additives according to customer specifications. Dipolen® boasts a high level of polyolefin purity, through an extremely selective recycling technology, and through thorough degassing and very fine filtration. Colors available are grey or black.

Information provided by MTM Plastics GmbH.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.935 g/cc0.0338 lb/in³ISO 1183
Moisture Absorption <= 0.100 %<= 0.100 %
Melt Flow  >= 2.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
>= 2.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
 >= 5.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
>= 5.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
 >= 10 g/10 min
@Load 5.00 kg,
Temperature 190 °C
>= 10 g/10 min
@Load 11.0 lb,
Temperature 374 °F
Ash <= 1.5 %<= 1.5 %Ignition Residue after 650°C; ISO 1172
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5858DIN 53505
Tensile Strength, Yield >= 22.0 MPa>= 3190 psi50 mm/min; ISO 527
Elongation at Yield >= 20 %>= 20 %50 mm/min; ISO 527
Tensile Modulus >= 0.950 GPa>= 138 ksi1 mm/min; ISO 527
Charpy Impact, Notched  >= 0.300 J/cm²
@Temperature -23.0 °C
>= 1.43 ft-lb/in²
@Temperature -9.40 °F
edgewise; ISO 179
 >= 0.600 J/cm²
@Temperature 23.0 °C
>= 2.86 ft-lb/in²
@Temperature 73.4 °F
edgewise; ISO 179

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem HD7255LS-L HDPE Injection Molding Polyethylene
Braskem Green PE SHC7260 Injection Molding High Density Polyethylene
Ravago Manufacturing Americas Echo® RPEHD NAT Recycled HDPE
RTP Company RTP 799 X 140537 High Density Polyethylene (HDPE); Cellulose Fiber - 95% Renewable Resource Content
Ravago Manufacturing Americas Echo® RPEHDW NAT (Injection) HDPE

PMTMP983 / 171620

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.