MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Niagara LaSalle 1144 Cold Finished Steel Bar
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: A high manganese, medium carbon, resulphurized steel with free machining qualities and higher mechanical properties than the lower carbon steels. This grade machines at 83% of 1212 with excellent as machined finish. It induction hardens satisfactorily, but the sulfides can contribute to quench cracking. It is difficult to weld.

Information provided by Niagra LaSalle Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 217217
Tensile Strength 745 MPa108000 psi
Tensile Strength, Yield 621 MPa90000 psi
Elongation at Break >= 10 %>= 10 %2"
Reduction of Area 30 %30 %
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 - 0.48 %0.40 - 0.48 %
Iron, Fe 97.5 - 98.01 %97.5 - 98.01 %as balance
Manganese, Mn 1.35 - 1.65 %1.35 - 1.65 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S 0.24 - 0.33 %0.24 - 0.33 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1144 Steel, as rolled
Niagara LaSalle Fatigue-Proof® Cold Finished Steel Bar
Niagara LaSalle StressProof® Cold Finished Steel Bar
AISI 1141 Steel, annealed at 815°C (1500°F)
AISI 1141 Steel, as rolled

NNIAL009 / 160299

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.