MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Polyalphaolefin
Categories: Polymer; Thermoplastic; Polyalphaolefin

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Polyalphaolefin". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.860 - 0.900 g/cc0.0311 - 0.0325 lb/in³Average value: 0.864 g/cc Grade Count:54
 0.740 - 0.740 g/cc
@Temperature 190 - 190 °C
0.0267 - 0.0267 lb/in³
@Temperature 374 - 374 °F
Average value: 0.740 g/cc Grade Count:38
Viscosity 2000 - 9000 cP2000 - 9000 cPAverage value: 3580 cP Grade Count:12
 400 - 1.16e+6 cP
@Temperature 190 - 190 °C
400 - 1.16e+6 cP
@Temperature 374 - 374 °F
Average value: 36400 cP Grade Count:60
Molecular Weight 7300 - 104000 g/mol7300 - 104000 g/molAverage value: 34300 g/mol Grade Count:14
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 43.0 - 94.043.0 - 94.0Average value: 71.9 Grade Count:9
Tensile Strength, Ultimate 0.200 - 9.00 MPa29.0 - 1310 psiAverage value: 1.71 MPa Grade Count:50
Elongation at Break 40.0 - 1200 %40.0 - 1200 %Average value: 524 % Grade Count:19
Shear Modulus 0.00200 - 0.0700 GPa0.290 - 10.2 ksiAverage value: 0.0145 GPa Grade Count:14
Penetration 3.00 - 28.03.00 - 28.0Average value: 16.6 Grade Count:17
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 60.0 - 139 °C140 - 282 °FAverage value: 97.3 °C Grade Count:31
Minimum Service Temperature, Air -37.0 - -20.0 °C-34.6 - -4.00 °FAverage value: -29.0 °C Grade Count:7
Glass Transition Temp, Tg -37.0 - -10.0 °C-34.6 - 14.0 °FAverage value: -26.2 °C Grade Count:64
Flash Point 235 °C455 °FAverage value: 235 °C Grade Count:39
Ring & Ball Softening Point 80.0 - 166 °C176 - 331 °FAverage value: 129 °C Grade Count:70
 
Processing PropertiesMetricEnglishComments
Pot Life 0.0833 - 15.0 min0.0833 - 15.0 minAverage value: 3.16 min Grade Count:36

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyether Block Amide (PEBA)
Evonik VESTOPLAST® 308 Amorphous Polyalphaolefin
Overview of materials for Styrene/Butadiene/Styrene (SBS)
Overview of materials for Ethylene Butyl Acrylate
Overview of materials for Polypropylene Copolymer

O4309 / 78317

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.