MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Saint-Gobain CHR® HM430 High Modulus PTFE Film Backing Acrylic Adhesive Pressure Sensitive Tape
Categories: Polymer; Tape

Material Notes: CHR® HM460 is manufactured from modified high-modulus PTFE film coated with high-temperature silicone adhesive.

Features/Benefits: The film of both CHR® HM430 and HM650 has been subjected to a special process that lowers its elongation and increases its breaking strength for easier handling. One side has an acrylic/silicone pressure sensitive adhesive and the other side offers low coefficient of friction film, which is thin and conformable. The backing offers excellent high temperature resistance and is chemically inert. This tape construction is weather resistant, stable and non-toxic. CHR® HM650 meets the requirements of MIL-I-23594C Type 1, Class 4.

Applications: CHR® HM430 and HM650 are often used as masking during metal bonding, roll covering on plastic extruders, and for fine wire harnesses. They are chosen for lay flat operations where anti-friction properties and solvent resistance are required.
Information provided by Saint Gobain Performance Products.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Elongation at Break 150 %150 %
Tear Strength 4.38 kN/m25.0 pliInitial Tear Strength
Peel Strength 0.270 kN/m1.54 pliAdhesion to Steel
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength 89.96 kV/mm2285 kV/in
Dielectric Breakdown 8000 V8000 V
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 177 °C350 °F
Minimum Service Temperature, Air -28.9 °C-20.0 °F
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Saint-Gobain CHR® M50 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® HM426 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Saint-Gobain CHR® HM350 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
NuSil R33-2186 Silicone Two Part Sealing & Adhesive
NuSil GEL-8150 Silicone Gel

PSTGQZ359 / 68873

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.