MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kureha KF Polymer 1550 High Viscosity PVDF Homopolymer
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: KF Polymer is a fire-resistant engineering plastic which maintains the excellent performance of a fluoropolymer. It shows well-balanced molding processability similar to general-purpose resins. KF polymer is being used in applications where heat resistance, anticorrosion, and weather-resistance are important.

Typical Applications:

  • Chemical valves, Pump part, & Fittings
  • Binder for lithium ion batteries
  • Hollow fiber for filtration of city water and sewage
  • Film & Sheet

Information provided by Kureha.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.77 - 1.79 g/cc0.0639 - 0.0647 lb/in³ASTM D792
Viscosity Test 150 cm³/g
@Temperature 30.0 °C
1.50 dl/g
@Temperature 86.0 °F
Inherent Viscosity in DMF Solution
Melt Flow 3.8 g/10 min
@Load 21.6 kg,
Temperature 230 °C
3.8 g/10 min
@Load 47.6 lb,
Temperature 446 °F
ASTM D1238
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1e+14 - 1e+15 ohm-cm1e+14 - 1e+15 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Melting Point 173 °C343 °FASTM D3418
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kureha KF Polymer 1000 PVDF Homopolymer
Kureha KF Polymer 1300 PVDF Homopolymer
Kureha KF Polymer 1100 PVDF Homopolymer
Kureha KF Polymer 850 PVDF Homopolymer
LG Chemical SEETEC H7411 Polypropylene, Homopolymer

PKUREHA93c / 150359

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.