Cadi C11000 ETP Standard Grade Copper
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
Material Notes:
The standard grade of copper - most widely used electrical conductor - suitable where mechanical design is not an issue and maximization of electrical or thermal conductivity is the primary concern.
Forms:
Rod
Bar
Plate
Information provided by Cadi Company.
Key Words:
ASTM B187, UNS C11000
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
8.91
g/cc
0.322
lb/in³
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell F
>= 80
@Diameter <=25.4 mm
>= 80
@Diameter <=1.00 in
hard temper
Electrical Properties
Metric
English
Comments
Electrical Resistivity
<=
0.00000176
ohm-cm
<=
0.00000176
ohm-cm
>98% IACS
Component Elements Properties
Metric
English
Comments
Copper, Cu
>= 99.9 %
>= 99.9 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO25 Temper flat products, tube
Eagle Brass 110 EPT COPPER, Annealed
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, OSO50 Temper flat products, rod, tube, shapes
Electrolytic Tough Pitch (ETP) Copper, UNS C11000, H00 Temper flat products
Eagle Brass 110 EPT COPPER, 1/4 Hard
NCADI01 / 15509
Free Trade Publications, Click Here!
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.