MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Edgetek® NL-20CF/000 Nylon 6/12, Carbon Fiber Reinforced  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 612 (PA612)

Material Notes:

Description/Features:

  • Carbon Fiber Reinforced

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.15 g/cc1.15 g/ccASTM D792
Water Absorption 0.24 %
@Thickness 3.17 mm
0.24 %
@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Water Absorption at Saturation 2.2 %
@Thickness 3.17 mm
2.2 %
@Thickness 0.125 in
Long-Term Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm0.0020 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 179 MPa26000 psiType 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 4.0 %4.0 %Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 276 MPa40000 psiASTM D790
Flexural Modulus 11.7 GPa1700 ksiASTM D790
Compressive Strength 145 MPa21000 psiASTM D695
Izod Impact, Notched 1.07 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
2.00 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 10000 ohm-cm10000 ohm-cmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 216 °C420 °FUnannealed, 0.125 in bars; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 213 °C415 °FUnannealed, 0.125 in bars; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit FRIANYL A63 CV10 Nylon 6.6 for injection molding, 10% carbon fiber reinforced
Celanese Nilit FRIANYL A63 CV30 Nylon 6.6 for injection molding, 30% carbon fiber reinforced
Avient Edgetek® NL-30CF/000 Nylon 6/12, Carbon Fiber Reinforced
Avient Edgetek® NN-15CF/000 Nylon 66 - 15% Carbon Fiber Reinforced
Avient Edgetek® NN-25CF/000 Nylon 6/6 - 25% Carbon Fiber

PH1PO0304 / 43475

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.