MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hostaform® S 9243 Impact Grade Acetal Copolymer
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM); Acetal Copolymer, Impact Modified

Material Notes: Description: Hostaform® Acetal Copolymers are a high strength, crystalline, thermoplastic engineering resins whose balance of properties and ease of processability offer performance and cost advantages over many other materials.

Specific Notes for this Grade: Injection molding grade with good low-temperature-impact strength. For parts requiring high impact energy absorption and excellent weld line strength.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.33 g/cc0.0480 lb/in³10x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %80x80x1mm, at 23°C and 50% RH; ISO 62
Water Absorption at Saturation 1.0 %1.0 %80x80x1mm, 23°C; ISO 62
Melt Flow 5.32 g/10 min
@Load 2.16 kg,
Temperature 190 °C
5.32 g/10 min
@Load 4.76 lb,
Temperature 374 °F
Calculated from Volume flow Rate: 4 cm3/10min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 105 MPa15200 psi30 sec value, 20x20x4 mm; ISO 2039, part 1; applied load 358 N
Tensile Strength, Yield 44.0 MPa6380 psimulti-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 50 mm/min
Elongation at Break >= 40 %>= 40 %multi-purpose specimen (ISO 3167); ISO 527, part 1/2; test speed 50 mm/min
Elongation at Yield 7.0 %7.0 %multi-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 50 mm/min
Tensile Modulus 2.10 GPa305 ksimulti-purpose test specimen (ISO 3167); ISO 527, part 1/2; test speed 1 mm/min
Flexural Modulus 2.00 GPa290 ksi80x10x4mm from multi-purpose test specimen (ISO 3167); ISO 178
Charpy Impact Unnotched 20.0 J/cm²
@Temperature -30.0 °C
95.2 ft-lb/in²
@Temperature -22.0 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eU
 NB
@Thickness 4.00 mm,
Temperature 23.0 °C
NB
@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eU
Charpy Impact, Notched 1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA
 1.40 J/cm²
@Thickness 4.00 mm,
Temperature 23.0 °C
6.66 ft-lb/in²
@Thickness 0.157 in,
Temperature 73.4 °F
80x10x4 m from multi-purpose test specimen (ISO 3167); ISO 179 1eA
Penetration 1010mm, deformation damage, 60x60x3mm; ISO 6603, part 2
 3030J, work to damage, 60x60x3 mm; ISO 6603, part 2
Tensile Creep Modulus, 1 hour 1800 MPa261000 psimulti-purpose test specimen (ISO 3167); ISO 899, part 1
Tensile Creep Modulus, 1000 hours 1000 MPa145000 psimulti-purpose test specimen (ISO 3167); ISO 899, part 1
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  3.8
@Frequency 100 Hz
3.8
@Frequency 100 Hz
80x80x1 mm; IEC 60250
 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
80x80x1 mm; IEC 60250
Dissipation Factor  0.0030
@Frequency 100 Hz
0.0030
@Frequency 100 Hz
80x80x1 mm; IEC 60250
 0.0060
@Frequency 1e+6 Hz
0.0060
@Frequency 1e+6 Hz
80x80x1 mm; IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 120 µm/m-°C
@Temperature 23.0 - 55.0 °C
66.7 µin/in-°F
@Temperature 73.4 - 131 °F
Longitudinal, 30x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 11359, part 1/2
Melting Point 166 °C331 °FDSC, 10 K/min, Molding compound; ISO 3146, method C1b
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C167 °F80x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 75, part 1/2
Vicat Softening Point 130 °C266 °FVST/B/50, 10x10x4 mm from multi-purpose test specimen (ISO 3167); ISO 306

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® S 9243 XAP2™ LS POM, Impact Modified
Celanese Hostaform® S 9243 XAP² ™ POM, Impact Modified
Delrin Delrin® 500T NC010 POM-I
Celanese Hostaform® C 9021 POM, Unfilled
Celanese Hostaform® C 52021 POM, Unfilled

PHCX31 / 46061

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.