Emerson & Cuming 24 Eccobond® Two-Component High Strength-Impact Resistant Epoxy Adhesive Clear, low viscosity, room temperature curing, epoxy adhesive. Exhibits resilient bonds when joining dissimilar materials. Excellent impact resistance. Recommended for bonding glass, polystyrene, polysulfone, polycarbonate, rigid PVC and PVDC. Mix ratio of 100:28. Cure Type: Room Temp or Heat Bonding Type: Epoxy The Eccobond® product line is now a part of Henkel; this specific grade is discontinued. |