MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chemtotal Manganese Oxide
Categories: Ceramic; Oxide

Material Notes: Manganese oxide is a prime source of manganese for which it is used in the manufacturing of steel and in cathodic material in dry-cell batteries. Manganese oxide is further processed and is known as MnO slug.

Information provided by Chemtotal

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Component Elements PropertiesMetricEnglishComments
CaO 5.0 - 8.0 %5.0 - 8.0 %
Carbon, C <= 0.030 %<= 0.030 %
Fe2O3 <= 1.5 %<= 1.5 %
MgO 4.0 - 6.0 %4.0 - 6.0 %
MnO 53 - 60 %53 - 60 %
Phosphorus, P <= 0.020 %<= 0.020 %
SiO2 21 - 25 %21 - 25 %
Sulfur, S <= 0.030 %<= 0.030 %
 
Descriptive Properties
A12O32.5 - 4.5%
Sieve Test100%Passing, 30 Mesh
 20-50%Passing, 200 Mesh
 65-75%Passing, 100 Mesh

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Evonik Rohacell® 200 WF High Heat Grade Polymethacrylimide (PMI) Foam
American Elements Manganese Oxide Nanopowder

PCHEMT027 / 194968

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.