MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Dow C702-20NA Polypropylene Impact Copolymer Resin  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer; Polypropylene, Impact Modified; Molded/Extruded

Material Notes:
    Overview
  • High impact performance
  • Contains a nucleating additive
  • Contains an antistatic additive
  • Complies with: U.S. FDA FCN 843, Canadian HPFB No Objection

DOW C702-20NA Polypropylene Resin is intended for use in injection molded applications requiring high impact resistance and good stiffness. The excellent moldability of this product enables short cycle times. It is particularly suited for industrial container, material handling, consumer products, and automotive applications.

Former Dow grade acquired by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D792
Melt Index of Compound 18 g/10 min
@Load 2.16 kg,
Temperature 230 °C
18 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 22.8 MPa3310 psiASTM D638
Elongation at Yield 4.5 %4.5 %ASTM D638
Flexural Modulus, 1% Secant 1210 MPa175000 psiASTM D790A
Izod Impact, Notched  0.747 J/cm
@Temperature -20.0 °C
1.40 ft-lb/in
@Temperature -4.00 °F
ASTM D256A
 0.854 J/cm
@Temperature 0.000 °C
1.60 ft-lb/in
@Temperature 32.0 °F
ASTM D256A
 1.87 J/cm
@Temperature 23.0 °C
3.50 ft-lb/in
@Temperature 73.4 °F
ASTM D256A
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C212 °FUnannealed; ASTM D648

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis RF366MO Polypropylene Random Copolymer for Injection Molding
Dow C702-20 Polypropylene Impact Copolymer Resin
Overview of materials for Polypropylene, Impact Modified; Molded/Extruded
Dow 6D43 Polypropylene Random Copolymer Resin
Dow 6D20 Polypropylene Random Copolymer Resin

PDOW0963 / 93299

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.