MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Formosa Plastics Formolene® 4181T Injection Molding Polypropylene  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Homopolymer with Antistat, ESCR Additives

Applications: For general purpose injection molding applications such as closures.

Formolene 4181T is a low viscosity, highly isotactic polypropylene homopolymer designed for various injection molded applications such as closures. It contains a unique combination of stabilizers which give it excellent processability with good stiffness, environmental stress crack resistance, heat performance and minimal odor and taste. Formolene 4181T contains antistat but no nucleation.

Meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Specimens were injection molded according to the conditions specified in ASTM D4101.

Information provided by Formosa Plastics Corporation, USA.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ASTM D1505
Melt Flow 30 g/10 min
@Temperature 230 °C
30 g/10 min
@Temperature 446 °F
I2; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 34.5 MPa5000 psi2" (50mm) per min.; ASTM D638
Elongation at Yield 9.0 %9.0 %2" (50mm) per min.; ASTM D638
Flexural Modulus, 1% Secant 1240 MPa180000 psi1.3 mm/min; ASTM D790
Izod Impact, Notched 0.214 J/cm0.400 ft-lb/inASTM D256
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Formosa Plastics Formolene® 4100N Injection Molding Polypropylene
Dow H103-00 Polypropylene Homopolymer
Formosa Plastics Formolene® 4100P Injection Molding Polypropylene
Formosa Plastics Formolene® 4100T Injection Molding Polypropylene
Formosa Plastics Formolene® 6502A Blow Molding and Injection Molding Polypropylene

PFPCPP21 / 38877

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.