MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company PermaStat® 600 Nat/Clear Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static - Transparent Grade - Violet Tint
Categories: Polymer; Thermoplastic; ABS Polymer

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.11 g/cc1.11 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
@Thickness 3.20 mm
0.0050 - 0.0070 in/in
@Thickness 0.126 in
ASTM D 955
Melt Flow 13 - 17 g/10 min
@Load 3.80 kg,
Temperature 230 °C
13 - 17 g/10 min
@Load 8.38 lb,
Temperature 446 °F
ASTM D 1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 38.6 MPa5600 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 1.86 GPa270 ksiASTM D 638
Flexural Strength 60.7 MPa8800 psiASTM D 790
Flexural Modulus 2.00 GPa290 ksiASTM D 790
Izod Impact, Notched 1.87 J/cm
@Thickness 3.20 mm
3.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched NB
@Thickness 3.20 mm
NB
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity <= 1.00e+10 ohm-cm<= 1.00e+10 ohm-cmASTM D 257
Surface Resistivity per Square <= 1.00e+11 ohm<= 1.00e+11 ohmASTM D 257; ESD STM11.11
Static Decay <= 2.0 sec<= 2.0 secFTMS101C; 4046.1
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C176 °FASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 72.8 °C163 °FASTM D 648
Flammability, UL94 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 199 - 238 °C390 - 460 °F
Mold Temperature 48.9 - 93.3 °C120 - 200 °F
Drying Temperature 82.2 °C
@Time 7200 sec
180 °F
@Time 2.00 hour
Moisture Content 0.10 %0.10 %
Dew Point -17.8 °C0.000 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PSI 3630 Medium Impact Polystyrene
RTP Company PermaStat® 600 MD Acrylonitrile Butadiene Styrene (ABS); ESD Protection - Permanently Anti-static - Transparent
RTP Company PermaStat® 600 Acrylonitrile Butadiene Styrene (ABS), ESD Protection - Permanently Anti-static
3M 2393 Premium High Temperature Masking Tape

PQZWA2593 / 91251

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.