MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Taiwan PU Corporation TPU-BH90 Hydrolysis Resistance, Blow Molding Polyether Base TPU
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Thermoplastic Polyurethane (TPU), Hydrolysis Resistance, Polyether Base, Blow Molding

Information provided by Taiwan PU Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9090
Tensile Strength at Break 31.38 MPa4551 psi
Elongation at Break 750 %750 %
100% Modulus 5.90 MPa
@Strain 100 %
856 psi
@Strain 100 %
300% Modulus 7.80 MPa
@Strain 300 %
1130 psi
@Strain 300 %
Resilience 4545%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 1010
 
Processing PropertiesMetricEnglishComments
Feed Temperature 180 °C356 °F
Middle Barrel Temperature 185 °C365 °FCompress zone
Front Barrel Temperature 190 °C374 °FMetering zone
Adapter Temperature 195 °C383 °F
Die Temperature 195 °C383 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Wanhua Chemical Wanthane® WHT-8290 Polyether-Based TPU
Taiwan PU Corporation TPU-BH85 Hydrolysis Resistance, Blow Molding Polyether Base TPU
Taiwan PU Corporation TPU-EH80 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Taiwan PU Corporation TPU-EH95 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Wanhua Chemical Wanthane® WHT-8285 Polyether-Based TPU

PTPU18 / 70874

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.