MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Owens Corning Glass Fiber Reinforced Polyurethane, Milled Fibers (RRIM), 13 wt.% glass
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Polyurethane, TS

Material Notes: Polyurethane is normally used for its structural properties when molded. It is highly resistant to most organic solvents. It is not recommended for use with strong acids and alkalis, steam, fuels, and ketones. Data provided by the manufacturer, Owens Corning.

Key Words: thermoset, fiber glass, fiberglass, fibreglass, fibre glass, FRP composites
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.07 g/cc0.0387 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 65 - 7565 - 75
Tensile Strength, Ultimate 19.0 MPa2760 psiASTM D638
Elongation at Break 140 %140 %ASTM D638
Flexural Modulus 0.310 GPa45.0 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
CTE, linear 140 µm/m-°C
@Temperature 20.0 °C
78.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ABSPC 9802 ABS/PC Molding Grade, High Impact, High Heat
Plastcom SLOVASTER® E GF 30 PBT, 30% glass fibre
Owens Corning Glass Fiber Reinforced Polyester (Pultruded), 55 wt.% glass
Owens Corning Glass Fiber Reinforced Polyurethane, Flaked Glass (RRIM), 23 wt.% glass
Covestro Baydur® SFR-243 Polyurethane Composite RRIM Foam, 15% Milled Glass Filled, MDI-based 2-Component Liquid System

POC008 / 55586

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.