MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2099 X 121240 C Biobased PLA-PC Hybrid Non Halogen Flame Retardant - 20% Bio-Content  (discontinued **)
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes:

Data for this product has not been recently verified, please contact RTP Company for more information before specifying this grade.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.22 g/cc1.22 g/ccASTM D 792
Linear Mold Shrinkage 0.0050 cm/cm
@Thickness 3.20 mm
0.0050 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.2 MPa8000 psiASTM D 638
Elongation at Break >= 10 %>= 10 %ASTM D 638
Tensile Modulus 2.76 GPa400 ksiASTM D 638
Flexural Strength 86.2 MPa12500 psiASTM D 790
Flexural Modulus 2.76 GPa400 ksiASTM D 790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.20 mm
1.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 13.3 J/cm
@Thickness 3.20 mm
25.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 65.6 °C150 °FASTM D 648
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 227 - 243 °C440 - 470 °F
Mold Temperature 26.7 - 40.6 °C80.0 - 105 °F
Drying Temperature 79.4 °C
@Time 14400 sec
175 °F
@Time 4.00 hour
Moisture Content 0.025 %0.025 %
Dew Point -40.0 °C-40.0 °F
Injection Pressure 68.9 - 138 MPa10000 - 20000 psi

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2099 X 121249 C Bio-Based Polylactic Acid (PLA); Standard Nucleator - Glass Fiber - 68% Renewable Resource Content
RTP Company RTP 2099 X 126216 D Bio-Based Polylactic Acid (PLA); Fast-Cycle Nucleator - Glass Fiber - 59% Renewable Resource Content
LATI Latilub 37 B01-02S Bio-Polymer
RTP Company RTP 2099 X 127618 R Bio-Based Polylactic Acid (PLA); PC-PLA Blend - Flame Retardant - Halogen Free - 20% Renewable Resource Content
RTP Company RTP 2099 X 126217 Z Bio-Based Polylactic Acid (PLA); Impact Modified - FDA Compliant Ingredients - 79% Renewable Resource Content

PQZVA15331 / 120524

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.