QLE 1100 is a 100% silicone solids elastomer designed for use as a conformal coating, but can also be used for cloth coating applications. Key Features: - 100% solids
- Transparent, ideal for pigmentation
- Fast cure at elevated temperatures
- Good abrasion resistance
- Primerless adhesion to many substrates
- Low viscosity
Part of the Amber Chemical Group. Data provided by manufacturer.Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017 |