MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES Luriblend® TPX-PA6/6-98020 40% Mineral Filled
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Mineral Filled; Nylon 66, PTFE Filled

Material Notes: Availability: North America

Forms: Pellets

Filler/Reinforcement: Mineral Fiber, 40% Filler by Weight

Additive: PTFE Lubricant(15%)

Features: Lubricated, Good Wear Resistance and Low Friction

Appearance: Black

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.60 g/cc0.0578 lb/in³ASTM D792
Water Absorption 0.50 %
@Time 86400 sec
0.50 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm
@Thickness 3.17 mm
0.0020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 105105ASTM D785
Tensile Strength, Yield 128 MPa18500 psiASTM D638
Elongation at Break 7.0 %7.0 %ASTM D638
Flexural Strength 152 MPa22000 psiASTM D790
Flexural Modulus 10.3 GPa1500 ksiASTM D790
Izod Impact, Notched 0.587 J/cm
@Thickness 3.17 mm
1.10 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 6.41 J/cm
@Thickness 3.17 mm
12.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Strength 17.7 kV/mm450 kV/inMethod A (Short-Time); ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 36.0 µm/m-°C20.0 µin/in-°FASTM D696
Melting Point 254 °C490 °F
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C490 °FUnannealed; ASTM D648
Flammability, UL94 HBHB

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
Techmer ES HiFill® TPX-HTN-01026 A 20% Glass Filled
Techmer ES Electrablend® TPX-PC-02071 Stainless Steel Fiber Filled
Overview of materials for Acrylic, General Purpose, Molded
Mitsui TPX® DX820 Methylpentene Copolymer

PTPC0911 / 136849

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.