MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexWeb® HRH-36/OX - 3/16 - 3.0 Para-Aramid/Phenolic Core
Categories: Other Engineering Material; Composite Core Material; Polymer; Thermoset; Aramid; Phenolic

Material Notes: Designation: Material-Cell Size (inches)-Density
HexWeb® HRH-36 is manufactured using KEVLAR® paper. The standard resin system is phenolic.

Features: Mechanical properties equivalent to KOREX®; Low moisture pickup; Excellent thermal stability; Smooth cell wall finish.
Applications: HexWeb® HRH-36 is a high performance non-metallic core, available in a wide range of densities, suitable for most composite sandwich applications. It can be readily heat formed to help produce complex components and offers similar mechanical properties to KOREX® core as well as comparable moisture pickup. In addition, HexWeb® HRH-36 offers a weight reduction over higher density NOMEX® honeycomb cores.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0481 g/cc0.00174 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Yield Strength 1.93 MPa280 psiBare
 2.07 MPa300 psiStabilized
Shear Modulus 0.0462 GPa6.70 ksiPlate Shear, L Direction
 0.0834 GPa12.1 ksiPlate Shear, W Direction
Shear Strength 0.896 MPa130 psiPlate Shear, L Direction
 1.07 MPa155 psiPlate Shear, W Direction

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexWeb® HDC-660 - 3/16 - 17.5 (R2) Heavy Density Core
Hexcel® HexWeb® HRH-36 - 1/8 - 4.0 Para-Aramid/Phenolic Core
Hexcel® HexWeb® HRH-36 - 1/8 - 3.0 Para-Aramid/Phenolic Core
Hexcel® HexWeb® HDC-G-327 - 3/16 - 15.0 (R2) Heavy Density Core
Hexcel® HexWeb® HDC - 3/16 - 16.0 (R2) Heavy Density Core

PHEXC365 / 98836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.