MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Multibase Multi-Flex® G 7430 TPE Styrene Ethylene Butylene Styrene Block Copolymer
Categories: Polymer; Thermoplastic

Material Notes:

Forms:

  • Pellets
  • Processing Methods:

  • Injection Molding
  • Information provided by Multibase

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Specific Gravity 0.942 g/cc0.942 g/ccASTM 792
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Shore A 727210 seconds; ASTM D2240
    Tensile Strength, Yield 12.8 MPa1850 psiElastic; ASTM D412
    Elongation at Break 750 %750 %Elastic; ASTM D412
    Tear Strength 29.8 kN/m170 pliASTM D624

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Multibase Multi-Flex® G 7155 TPE Styrene Ethylene Butylene Styrene Block Copolymer
    Multibase Multi-Flex® G 7150 TPE Styrene Ethylene Butylene Styrene Block Copolymer
    Multibase Multi-Flex® G 7680 TPE Styrene Ethylene Butylene Styrene Block Copolymer
    Multibase Multi-Flex® G 7940 TPE Styrene Ethylene Butylene Styrene Block Copolymer
    Covestro Desmopan® 3491A Polyurethane

    PMULTI084 / 53988

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.