MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Axiall UV-6676 Rigid PVC, Molding  (discontinued **)
Categories: Polymer; Thermoplastic; Vinyl (PVC)

Material Notes: Georgia Gulf UV-6676 is a weatherable, high flow injection molding compound, specially formulated for outdoor UV exposure. This compound was designed to be used in various accessory parts, such as fence post caps, rain gutter parts, deck parts, etc.

Information provided by Georgia Gulf

Georgia Gulf became Axiall Corporation, which was later acquired by Westlake Plastics. This specific grade is discontinued.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.40 g/cc1.40 g/ccASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm0.0030 - 0.0040 in/inASTM D-955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D-785
Tensile Strength, Yield 40.0 MPa5800 psiASTM D-638
Tensile Modulus 2.21 GPa320 ksiASTM D-638
Flexural Strength 65.5 MPa9500 psiASTM D-790
Flexural Modulus 2.28 GPa330 ksiASTM D-790
Izod Impact, Notched  0.534 J/cm
@Thickness 3.17 mm,
Temperature -20.0 °C
1.00 ft-lb/in
@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
 9.61 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
18.0 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 14.7 J
@Temperature 23.0 °C
10.8 ft-lb
@Temperature 73.4 °F
1/2" R Tup, 65 mil
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 72.00 °C161.6 °FASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C158 °FASTM D-648
Flammability, UL94 5VA5VA
Oxygen Index 35 %35 %ASTM D-2863
 
Descriptive Properties
Flow Ratio (Distance/Wall Thickness, 390-400°F)230Georgia Gulf Test
UL Weatherability Rating F(2)UL-746C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Axiall UV-6670 Rigid PVC, Molding
Axiall UV-6680 Rigid PVC, Molding
Axiall UV-6685 Rigid PVC, Molding
Axiall 1601 Clear 7002 Flexible PVC
Axiall 8150 Rigid PVC, Extrusion & Molding

PGGUL461 / 41737

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.