MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Clariant Remafin PP1100NAT Polypropylene Impact Modified Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes:

Data provided by Clariant Masterbatches

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.900 g/cc0.900 g/ccASTM D792
Melt Flow 18 g/10 min18 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 21.0 MPa3050 psiASTM D638
Elongation at Break 8.0 %8.0 %ASTM D638
Flexural Modulus 0.800 GPa116 ksiASTM D790
Izod Impact, Notched 1.02 J/cm1.91 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 76.1 °C169 °FASTM D648
 
Processing PropertiesMetricEnglishComments
Melt Temperature 191 - 221 °C375 - 430 °F
Mold Temperature 37.8 - 65.6 °C100 - 150 °F
Injection Pressure 4.96 - 8.27 MPa720 - 1200 psiSecondary
 8.27 - 13.8 MPa1200 - 2000 psiInitial
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi
Shot Size 30 - 80 %30 - 80 %
Screw Speed 20 - 100 rpm20 - 100 rpm

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Clariant Remafin PESP0006 High Density Polyethylene, 10% Glass Fiber
Celanese Zytel® ST801 NC010A PA66-HI
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade
Sumitomo Chemical ESPOLEX® WT361 Thermoplastic Elastomer

PCLAR170 / 82295

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.