MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Purell EP274P Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Purell EP274P is a nucleated polypropylene impact copolymer suitable for use in injection molding applications. Purell EP274P exhibits an excellent balance of stiffness and low – temperature toughness. Purell EP274P is typically used in injection molding applications to produce medical products where high mechanical properties are required. Applications: Healthcare Applications, Medical Devices

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.900 g/cc0.0325 lb/in³ISO 1183-1
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 230 °C
15 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133-1
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 45.0 MPa6530 psiISO 2039-1
Tensile Strength, Yield 20.0 MPa2900 psiISO 527-1,-2
Elongation at Break >= 50 %>= 50 %ISO 527-1,-2
Elongation at Yield 7.0 %7.0 %ISO 527-1,-2
Tensile Modulus 0.950 GPa138 ksiISO 527-1,-2
Charpy Impact, Notched  0.500 J/cm²
@Temperature -20.0 °C
2.38 ft-lb/in²
@Temperature -4.00 °F
Type 1, Edgewise, Notch A; ISO 179
 0.800 J/cm²
@Temperature 0.000 °C
3.81 ft-lb/in²
@Temperature 32.0 °F
Type 1, Edgewise, Notch A; ISO 179
 1.30 J/cm²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
Type 1, Edgewise, Notch A; ISO 179
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 78.0 °C172 °Funannealed; ISO 75B-1,-2
Vicat Softening Point 142 °C288 °FA50; ISO 306
 
Descriptive Properties
Ball Indentation Hardness (MPa)H358/30
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Purell 2410T Linear Low Density Polyethylene (LLDPE), Blow Molding Grade
Covestro Makrolon® 2807 MAS 167 Polycarbonate
Covestro Makrolon® 2405 MAS048 Polycarbonate
Advanced Elastomer Systems Santoprene® 281-73 Thermoplastic Rubber
Zylog Hipolyene® 8021 HC Thermoplastic Polyolefin & PP Compound

PEQT8618 / 220252

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.