MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Ineos ABS Lustran® M203FC  (discontinued **)
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Molded

Material Notes: Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,

Property data per ISO test methods.

This product was transitioned to the INEOS Styrolution Novodur® trade name. Information provided by the manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 g/cc0.0379 lb/in³
Melt Flow 33 g/10 min
@Load 10.0 kg,
Temperature 220 °C
33 g/10 min
@Load 22.0 lb,
Temperature 428 °F
Estimated using room temperature density
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 46.0 MPa6670 psi
Elongation at Yield 2.6 %2.6 %
Tensile Modulus 2.40 GPa348 ksi
Charpy Impact Unnotched 11.0 J/cm²52.4 ft-lb/in²
 9.00 J/cm²
@Temperature -30.0 °C
42.8 ft-lb/in²
@Temperature -22.0 °F
Charpy Impact, Notched 1.50 J/cm²7.14 ft-lb/in²
 0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity >= 1.00e+15 ohm-cm>= 1.00e+15 ohm-cm
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohm
Dielectric Constant  2.9
@Frequency 1e+6 Hz
2.9
@Frequency 1e+6 Hz
 3.0
@Frequency 100 Hz
3.0
@Frequency 100 Hz
Dielectric Strength 35.0 kV/mm889 kV/in
Dissipation Factor  0.0050
@Frequency 100 Hz
0.0050
@Frequency 100 Hz
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
Comparative Tracking Index 600 V600 V
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C
@Temperature 20.0 °C
50.0 µin/in-°F
@Temperature 68.0 °F
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °F
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °C201 °F
Vicat Softening Point 99.0 °C210 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution Novodur® M203FC ABS
Celanese Crastin® SC164 NC010 PBT
Celanese Celanex® 2402 MT PBT, Medical Technology
Covestro Makrolon® 2858 Polycarbonate, Injection Grade
Covestro Makrolon® 2458 Polycarbonate, Injection Grade

PLANX639 / 49954

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.