MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kolon KOPA® KN333 Heat Resistant Nylon 66  (discontinued **)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Heat Stabilized

Material Notes: KOPA® is a thermoplastic resin with excellent mechanical, thermal and electrical properties and is widely used in the automobile, electrical and industrial parts.

High tensile strength, outstanding self lubrication and abrasion resistance, excellent chemical & weather resistance, high usage temperature

Information provided by US distributor, API-Kolon.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.14 g/cc0.0412 lb/in³DIN 53479; ASTM D792
Water Absorption 1.3 %1.3 %DIN 53475; ASTM D570
Linear Mold Shrinkage 0.011 - 0.013 cm/cm0.011 - 0.013 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120DIN 53505; ASTM D785
Tensile Strength, Ultimate 85.3 MPa12400 psiDIN 53455; ASTM D638
Elongation at Break 40 %40 %DIN 53455; ASTM D638
Flexural Yield Strength 132 MPa19200 psiDIN 53455; ASTM D790
Flexural Modulus 2.94 GPa427 ksiDIN 53452; ASTM D790
Izod Impact, Notched 0.588 J/cm1.10 ft-lb/inDIN 53453; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.3
@Frequency 1e+6 Hz
3.3
@Frequency 1e+6 Hz
ASTM D150/DIN 53483
Dielectric Strength 20.0 kV/mm508 kV/inASTM D149/DIN 53481
Arc Resistance 128 sec128 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
DIN 53752; ASTM D696
Melting Point 255 °C491 °FDIN 53736; ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 235 °C455 °FDIN 53461; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C185 °FDIN 53461; ASTM D648
Flammability, UL94 V-2V-2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Polyplastics Duracon® M90-71 Acetal Co-polymer (POM), Heat resistance
Celanese Hostaform® MT8U05 POM, Medical Technology
Celanese Hostaform® MT8F02 POM, Medical Technology
Celanese Hostaform® MT8F01 POM, Medical Technology
Celanese Hostaform® MT24F01 POM, Medical Technology

PKOL034 / 48940

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.