MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Petrothene GA578189 Linear Low Density Polyethylene (LLDPE), Injection Molded  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Petrothene GA578189 is a pelletized LLDPE resin for injection molding applications such as lids, caps and closures, containers and other items needing rigidity and good appearance. GA578189 can be used in operations requiring fast cycle times, as well. Applications: Caps & Closures, Containers, Housewares, Lids, Outdoor and Power Tools

Information provided by LyondellBasell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.928 g/cc0.0335 lb/in³ASTM D1505
Melt Flow 85 g/10 min
@Load 2.16 kg,
Temperature 190 °C
85 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Spiral Flow 56.0 cm22.0 inLYB Method
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 5454ASTM D2240
Tensile Strength at Break 13.0 MPa1890 psiASTM D638
Tensile Strength, Yield 17.0 MPa2470 psiASTM D638
Elongation at Yield 10 %10 %ASTM D638
Flexural Modulus, 1% Secant 560 MPa81200 psiASTM D790
2% Secant Modulus 0.480 GPa69.6 ksiASTM D790
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 50.0 °C122 °Funannealed; ASTM D648
Vicat Softening Point 85.0 °C185 °FASTM D1525
Brittleness Temperature -60.0 °C-76.0 °FASTM D746
 
Descriptive Properties
Processing MethodInjection Molding

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Petrothene GA574200 Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene GA584189 Linear Low Density Polyethylene (LLDPE), Injection Molded
LyondellBasell Petrothene GA623119 Linear Low Density Polyethylene (LLDPE)/Hexene, Molded
Dow DOWLEX™ 2267G Linear Low Density Polyethylene
Dow DNDA-9810 NT 7 Linear Low Density Polyethylene Resin

PEQT8824 / 220458

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.