MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Avient Edgetek® XP9242701 Polyphenylene Sulfide (PPS)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: Injection Speed: 50 to 80% Holding Time: 3 to 9 sec Injection Time: 1 to 3 sec Cycle Time: 18 to 70 sec

Information provided by PolyOne

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.65 g/cc1.65 g/ccASTM D792
Filler Content 10 %10 %Carbon Fiber Reinforcement
 30 %30 %Glass Fiber Reinforcement
Linear Mold Shrinkage, Flow 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 258 MPa37400 psiASTM D638
Flexural Modulus 18.0 GPa2610 ksiASTM D790
Charpy Impact, Notched 60.0 J/cm²286 ft-lb/in²J/m; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Surface Resistance <= 1.00e+9 ohm<= 1.00e+9 ohmASTM D257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FUnannealed; ASTM D648
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
UL 94
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 270 - 280 °C518 - 536 °F
Middle Barrel Temperature 290 - 330 °C554 - 626 °F
Front Barrel Temperature 290 - 330 °C554 - 626 °F
Nozzle Temperature 280 - 320 °C536 - 608 °F
Mold Temperature 120 - 150 °C248 - 302 °F
Drying Temperature 130 - 150 °C266 - 302 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Injection Pressure 70.0 - 100 MPa10200 - 14500 psi
Hold Pressure 50.0 - 80.0 MPa7250 - 11600 psi
Back Pressure 1.00 - 2.50 MPa145 - 363 psi
Screw Speed 80 - 120 rpm80 - 120 rpm
 
Descriptive Properties
FormsPellets
Generic MaterialPPS
Generic NamePolyphenylene Sulfide (PPS)
Processing MethodInjection Molding
Regional AvailabilityAsia Pacific

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® CP-0301 Fiber Compound
Mocom (ALBIS) Tedur® L 9200-1 Polyphenylene Sulfide
Evonik PROCON™ PPS Polyphenylene Sulfide
DuPont Mobility and Materials VESPEL TP-8474 Polyimide
Celanese Fortron® 4184 L6 Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled

PH0POL1312 / 145881

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.