MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Celanex® 3114 7.5% Fiberglass Reinforced Polybutylene Terephthalate
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled

Material Notes: Description: Celanex 3114 is a flame retarded, nonexuding, 7.5% glass reinforced polybutylene terephthalate providing a good balance of mechanical and electrical properties. This grade is rated UL94 V-0 down to 1/32 inch thickness and is recommended for all electrical/electronic applications.

Information provided by Celanese Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.49 g/cc0.0538 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 67.0 MPa9720 psi5 mm/min; ISO 527-2/1A
Tensile Modulus 5.10 GPa740 ksi1 mm/min; ISO 527-2/1A
Flexural Modulus 4.10 GPa595 ksiISO 178
Charpy Impact, Notched 0.290 J/cm²1.38 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmIEC 60093
Surface Resistance >= 1.00e+17 ohm>= 1.00e+17 ohmIEC 60093
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
 
Thermal PropertiesMetricEnglishComments
Melting Point 225 °C437 °FISO 11357-1,2,3
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 230 - 240 °C446 - 464 °F
Middle Barrel Temperature 235 - 250 °C455 - 482 °F
Front Barrel Temperature 240 - 255 °C464 - 491 °F
Nozzle Temperature 250 - 255 °C482 - 491 °F
Melt Temperature 250 - 255 °C482 - 491 °F
Mold Temperature 65.0 - 93.0 °C149 - 199 °F
Drying Temperature 121 °C250 °F
Dry Time 4 hour4 hour
Back Pressure 0.000 - 0.345 MPa0.000 - 50.0 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Nilit Nilitop BT G6 FR C3 is a 30% Glass Fiber Reinforced, Flame Retardant PBT
Celanese Coolpoly® D4302 Thermally Conductive Polybutylene Terephthalate

PHCV94 / 45935

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.