MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman Diamond ASA M806 ASA Weatherable Polymers Direct Metallizable Grade, Medium Heat
Categories: Polymer; Thermoplastic; ASA Polymer; Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded

Material Notes:

A. Schulman has acquired Network Polymers & Diamond Polymers.

Key Words: Acrylonitrile Styrene Acrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.08 g/cc1.08 g/ccASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm0.0040 - 0.0070 in/inASTM D955
Melt Flow 22 g/10 min
@Load 10.0 kg,
Temperature 240 °C
22 g/10 min
@Load 22.0 lb,
Temperature 464 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 51.8 MPa7510 psichs 2.0 in/min; ASTM D638
Flexural Modulus 2.377 GPa344.8 ksitangent; chs 0.05 in/min; ASTM D790
Izod Impact, Notched 0.530 J/cm
@Thickness 6.35 mm,
Temperature 23.0 °C
0.992 ft-lb/in
@Thickness 0.250 in,
Temperature 73.4 °F
ASTM D256

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman Diamond ASA M-143
A. Schulman Diamond ASA 91802
A. Schulman Diamond ASA 5946
A. Schulman Diamond ASA S124 ASA Weatherable Polymers Injection Molding Grade, Medium Modulus
A. Schulman Diamond ASA M-523

PDIAM338 / 126429

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.