MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient PolyOne® CPE 30-2 Chlorinated Polyethylene (CPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes:

An excellent choice for low-voltage power-and-cable control cables, this filled, flexible thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of thermoplastic extrusion processing without the need to invest in continuous vulcanization (CV) equipment. CPE 30-2 provides better limiting oxygen index performance, as well as good elongation at lower use temperatures. Good moisture, oil and electrical properties.

Applications:

  • Power and Control Cable Jacket

Market:

  • Wire & Cable
PolyOne First Choice

Disclaimer: Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment.
Note: Pre-drying is recommended for 8-24 hours at 175°-185°F.
NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.36 g/cc1.36 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 464610 sec; ASTM D2240
Tensile Strength, Ultimate 10.3 MPa1500 psiType 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 350 %350 %Type 4 - Flexibles, 20 in/min; ASTM D638
Tensile Modulus 0.00689 GPa1.00 ksiType 4 - Flexibles, 20 in/min; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -35.0 °C-31.0 °FASTM D746
Oxygen Index 32 %32 %0.075 in; ASTM D2863
 
Descriptive Properties
AppearancePellets/CubesASTM D2090

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient FireCon™ CPE 30-2 RoHS BLACK Polyethylene, Chlorinated (CPE)
Avient FireCon™ CPE 30-2 Natural Chlorinated Polyethylene (CPE)
Dow Tyrin® 3615P Chlorinated Polyethylene Elastomer

PH1PO3452 / 45084

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.