MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Chevron Phillips Marlex® 9514H Polyethylene; HDPE  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: High density polyethylene. This gas phase, high molecular weight hexene copolymer is tailored for lightweight blow molded applications that:
  • Require excellent stiffness to ESCR ratio
  • Require good melt strength
  • Are durable and recyclable for sustainability

Applications: Typical blow molded applications for 9514H include:

  • Household and industrial chemical containers
  • Large parts

Information provided by Phillips

This resin meets these specifications:

  • ASTM D4976 - PE 235
  • FDA 21 CFR 177.1520(c) 3.2a, use conditions B through H per 21 CFR 176.170(c)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.957 g/cc0.0346 lb/in³ASTM D-1505
ESCR 100% Igepal® 50 hour50 hourCondition B, F50; ASTM D-1693
Melt Index of Compound 0.30 g/10 min
@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D-1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 30.0 MPa4350 psi2 in/min, Type IV bar; ASTM D-638
Elongation at Break 800 %800 %2 in/min, Type IV bar; ASTM D-638
Flexural Modulus 1.41 GPa205 ksiTangent - 16:1 span:depth, 0.5 in/min; ASTM D-790
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -75.0 °C<= -103 °FType A, Type I specimen; ASTM D-746

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Chevron Phillips Marlex® 9018 HDPE Injection Molding Resin
Chevron Phillips Marlex® 1007 Injection Molding Resin
Chevron Phillips Marlex® 1009 LDPE Injection Molding Resin
Chevron Phillips Marlex® 1122B Injection Molding Resin
Chevron Phillips Marlex® 1003 LDPE Injection Molding Resin

PCHEVD237 / 20731

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.