MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Goodfellow Reduced Graphene Oxide (GO) Powder
Categories: Carbon

Material Notes: Reduced graphene oxide is obtained by reducing graphene oxide chemically, thermally, or by irradiation to get the powder form.

Excellent conductivity. Odorless. Dispersible in low concentrations (<0.1 mg/mL) in DMF, DMSO, NMP. Applications: Biomedical, batteries, printable graphene electronics, supercapacitors.

Information provided by Goodfellow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.91 g/cc0.0690 lb/in³
Moisture Absorption 3.70 - 4.20 %3.70 - 4.20 %
Particle Size 260 - 295 µm260 - 295 µmz-sized in NMP at 0.1 mg/mL
Specific Surface Area 423 - 500 m²/g423 - 500 m²/gBET
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.150 ohm-cm0.150 ohm-cm20 nm thick film
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 77 - 87 %77 - 87 %
Hydrogen, H 0.0 - 1 %0.0 - 1 %
Nitrogen, N 0.0 - 1 %0.0 - 1 %
Oxygen, O 13 - 22 %13 - 22 %
Sulfur, S 0.0 %0.0 %
 
Descriptive Properties
ColorBlack

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Goodfellow Graphene Oxide (GO) Film
Goodfellow Graphene Oxide (GO) Dispersion
Goodfellow CVD Graphene Film on Quartz Glass
Goodfellow HDPlas® GNP Plasma Functionalized Graphene Nanoplatelets
Goodfellow CVD Graphene Film on Copper Foil

CGOODF099j / 197461

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.