MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Teijin Panlite® L-1225ZL Polycarbonate, Weather Resistant  (discontinued **)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, UV Stabilized

Material Notes: Injection Molding.

Applications: Ulta-thin lamp lenses.

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Water Absorption 0.20 %0.20 %23°C; 24 hr; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7777ASTM D785
Tensile Strength, Ultimate 64.0 MPa9280 psiASTM D638
Tensile Strength, Yield 65.0 MPa9430 psiASTM D638
Elongation at Break 130 %130 %ASTM D638
Elongation at Yield 6.0 %6.0 %ASTM D638
Tensile Modulus 2.19 GPa318 ksiASTM D638
Flexural Yield Strength 96.0 MPa13900 psiASTM D790
Flexural Modulus 2.33 GPa338 ksiASTM D790
Compressive Yield Strength 77.0 MPa11200 psiASTM D695
Izod Impact, Notched  0.500 J/cm
@Thickness 6.40 mm
0.937 ft-lb/in
@Thickness 0.252 in
ASTM D256
 1.00 J/cm
@Thickness 3.20 mm
1.87 ft-lb/in
@Thickness 0.126 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 3.00e+16 ohm-cm3.00e+16 ohm-cmASTM D257
Dielectric Constant  2.9
@Frequency 60 Hz
2.9
@Frequency 60 Hz
ASTM D150
 2.95
@Frequency 1e+6 Hz
2.95
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 30.0 kV/mm
@Thickness 1.60 mm
762 kV/in
@Thickness 0.0630 in
quick pressure rise method; ASTM D149
Dissipation Factor  0.00040
@Frequency 60 Hz
0.00040
@Frequency 60 Hz
ASTM D150
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 100 sec100 secASTM D495
Comparative Tracking Index 300 V300 VIEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature 20.0 °C
38.9 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 138 °C280 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 128 °C262 °FASTM D648
UL RTI, Electrical 125 °C
@Thickness 1.47 mm
257 °F
@Thickness 0.0579 in
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.47 mm
239 °F
@Thickness 0.0579 in
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.47 mm
257 °F
@Thickness 0.0579 in
Flammability, UL94  V-2
@Thickness 1.47 mm
V-2
@Thickness 0.0579 in
 V-2
@Thickness 3.05 mm
V-2
@Thickness 0.120 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.5851.585ASTM D542
Transmission, Visible 88 %
@Thickness 3.00 mm
88 %
@Thickness 0.118 in
ASTM D1003

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Teijin Panlite® L-1225Z Polycarbonate, Weather Resistant
Teijin Panlite® L-1225 Polycarbonate, Standard Grade
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Teijin Panlite® L-1225LM Polycarbonate
Teijin Panlite® L-1225L Standard (mold release/ice color grade) Polycarbonate Resin

PLAT14 / 49994

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.