MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

VICTREX ST™ P45 PolyEtherKetoneEtherKetoneKetone (PEKEKK)
Categories: Polymer; Thermoplastic; Polyketone

Material Notes: High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, coarse powder for extrusion compounding, low flow, color natural.

Information Provided by Victrex.

Vendors: Victrex is a global leader in high-performance PEEK and PAEK polymers, transforming industries from aerospace to medical devices. For 40 years, our innovative polymer solutions help customers achieve new levels of performance, sustainability, and cost efficiency across applications that millions rely on daily from smartphones to aircraft components. As pioneers in polymer engineering, we're committed to delivering transformational solutions that address global materials challenges. Visit www.victrex.com, call (800) VICTREX /1-484-342-6001, or email victrexplc@victrex.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³Crystalline; ISO 1183
Viscosity 225000 cP
@Temperature 420 °C
225000 cP
@Temperature 788 °F
melt; ISO 11443
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 110 MPa16000 psiISO 527
Elongation at Break 10 %10 %ISO 527
Tensile Modulus 4.20 GPa609 ksiISO 527
Flexural Strength 170 MPa24700 psiISO 178
Flexural Modulus 4.00 GPa580 ksiISO 178
Izod Impact, Notched (ISO) 5.00 kJ/m²2.38 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) NBNBISO 180/U
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg 162 °C324 °FOnset; ISO 11357
 169 °C336 °FMidpoint; ISO 11357
 
Processing PropertiesMetricEnglishComments
Processing Temperature 410 - 420 °C770 - 788 °F
Dry Time  3.00 hour
@Temperature 180 °C
3.00 hour
@Temperature 356 °F
 6.00 hour
@Temperature 150 °C
6.00 hour
@Temperature 302 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ensinger Tecapeek® ST PolyEtherKetoneEtherKetoneKetone, Unreinforced
Overview of materials for Polyetheretherketone, Unreinforced
VICTREX ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced
Gharda Chemicals G-PAEK™ 1200G Ultra High Performance PEK Polymer
RTP Company RTP 3999X56542A Polyetherketoneetherketoneketone (PEKEKK), Wear Resistant

PVICTB10d / 172232

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.