MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Eagle Brass 762 Nickel Silver 12%, Annealed
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: 762 is a nickel silver alloy that has excellent strength, stress relaxation resistance, and solderability. Due to it being extremely resistant to corrosion it doesn't tarnish easily and has a long shelf life. Typical uses include springs for relays, condensers, and decorative belt buckles.

Information provided by Eagle Brass Company

Key Words: UNS C76200, ASTM B122
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.58 g/cc0.310 lb/in³Annealed
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell 30T 44 - 6744 - 67Thickness > 0.020 Inch
Tensile Strength, Ultimate 393 - 517 MPa57000 - 75000 psi
Tensile Strength, Yield 145 - 352 MPa21000 - 51000 psi0.2% offset
Elongation at Break 32 - 49 %32 - 49 %in 2 in.
Tensile Modulus 124 GPa18000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000198 ohm-cm0.0000198 ohm-cmAnnealed
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Thermal Conductivity 41.5 W/m-K288 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 59 %59 %
Nickel, Ni 12 %12 %
Zinc, Zn 29 %29 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Nickel silver 65-12, UNS C75700, H06Temper sheet or strip
Eagle Brass 762 Nickel Silver 12%, Hard
Nickel silver 55-18, UNS C77000
Nickel silver 55-18, UNS C77000, H04 Temper flat products
Leaded Nickel Bronze, UNS C97600, Copper Casting Alloy

NEAGLE209 / 147458

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.