MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded; Polyurethane, TP

Material Notes:
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.29 g/cc1.29 g/ccASTM D792
Linear Mold Shrinkage  0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
48 hr, at 80 and 121°C; ASTM D955
 0.0010 - 0.0030 cm/cm
@Thickness 3.20 mm
0.0010 - 0.0030 in/in
@Thickness 0.126 in
72 hr; ASTM D955
 0.0020 - 0.0040 cm/cm
@Thickness 3.20 mm
0.0020 - 0.0040 in/in
@Thickness 0.126 in
48 hr at 121°C; ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 656515 sec delay; ASTM D2240
Tensile Strength, Ultimate 35.0 MPa5080 psiat max load; ASTM D638
Elongation at Break 30 %30 %ASTM D412
Flexural Modulus 0.900 GPa131 ksiat 70°C, tangent
 1.40 GPa203 ksitangent; ASTM D790
Izod Impact, Notched 2.00 J/cm3.75 ft-lb/inASTM D256
Falling Dart Impact 6.01 J4.43 ft-lbat -30°C; ASTM D3029
Tear Strength 110 kN/m628 pliASTM D624
 
Thermal PropertiesMetricEnglishComments
CTE, linear 27.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
15.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
2.7 mm/mm; ASTM D696
Melting Point 220 °C428 °Fby DSC, 10°C per 220 minutes
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C
@Thickness 3.20 mm
194 °F
@Thickness 0.126 in
ASTM D648
 
Descriptive Properties
Heat Sag 15 mmASTM D3769, 1 hr, at 121°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A. Schulman POLYPUR™ FPU 1380 Thermoplastic Polyurethane Compound
Covestro Desmopan® W DP 89051D Polyurethane
Lubrizol Estane® 2103-55D Thermoplastic Polyurethane Elastomer
A. Schulman POLYPUR™ FPU 1156 Thermoplastic Polyurethane
A. Schulman POLYPUR™ FPU 1103F Thermoplastic Polyurethane Compound

PASHU272 / 25236

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.