MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Albis Plastics Polyethylene PE 11A GF30-001 30% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE)

Material Notes: Semi-crystalline Polyethylene (PE)

Characteristics: High Stiffness and Chemical Resistance

Applications: Appliances, Cases, Furniture, Housewares, Luggage and Packaging

Processing: Injection Molding (Melt Temperature: 410-575°F, Mold Temperature: 40-160°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.17 g/cc0.0423 lb/in³ASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.4 MPa3390 psiASTM D638
Elongation at Break 10.7 %10.7 %ASTM D638
Modulus of Elasticity 3.51 GPa509 ksiASTM D638
Flexural Yield Strength 26.2 MPa3800 psiASTM D790
Flexural Modulus 3.02 GPa438 ksiASTM D790
Izod Impact, Notched 0.720 J/cm1.35 ft-lb/inASTM D256
 
Processing PropertiesMetricEnglishComments
Melt Temperature 210 - 302 °C410 - 576 °FInjection
Mold Temperature 4.00 - 71.0 °C39.2 - 160 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Albis Plastics Polyethylene PE 11A GF20-001 20% Glass Fiber
Techmer ES HiFill® HDPE GF30 30% Glass Filled
Omni Plastics OmniTech™ HDPE GRC30 High Density Polyethylene, 30% Glass Reinforced
Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled
RTP Company RTP 705 Z  High Density Polyethylene (HDPE) Glass Fiber 30% - FDA Type

PZA1B63 / 21750

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.