MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

RTP Company RTP 2501 FR Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber - Flame Retardant - Non-PBBO/E - UL94 V-0
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Glass Fiber Filled; Polycarbonate (PC)

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.27 g/cc1.27 g/ccASTM D 792
Water Absorption 0.10 %
@Time 86400 sec
0.10 %
@Time 24.0 hour
ASTM D 570
Additive Loading 10 %10 %Primary Additive
Linear Mold Shrinkage 0.0030 - 0.0050 cm/cm
@Thickness 3.20 mm
0.0030 - 0.0050 in/in
@Thickness 0.126 in
ASTM D 955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 118118ASTM D 785
Tensile Strength at Break 68.9 MPa10000 psiASTM D 638
Elongation at Break 3.0 - 4.0 %3.0 - 4.0 %ASTM D 638
Tensile Modulus 4.83 GPa700 ksiASTM D 638
Flexural Strength 124 MPa18000 psiASTM D 790
Flexural Modulus 4.48 GPa650 ksiASTM D 790
Izod Impact, Notched 0.801 J/cm
@Thickness 3.20 mm
1.50 ft-lb/in
@Thickness 0.126 in
ASTM D 256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.20 mm
10.0 ft-lb/in
@Thickness 0.126 in
ASTM D 4812
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+16 ohm-cm>= 1.00e+16 ohm-cmASTM D 257
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 132 °C270 °FASTM D 648
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Melt Temperature 243 - 274 °C470 - 525 °F
Mold Temperature 51.7 - 93.3 °C125 - 200 °F
Drying Temperature 93.3 °C
@Time 14400 sec
200 °F
@Time 4.00 hour
Moisture Content 0.020 %0.020 %
Dew Point -28.9 °C-20.0 °F
Injection Pressure 68.9 - 103 MPa10000 - 15000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
RTP Company RTP 2501 Polycarbonate/ABS Alloy (PC/ABS), Glass Fiber
RTP Company RTP 2501 A  Polycarbonate/ABS Alloy (PC/ABS) Glass Fiber 10%
Polymer Resources PC/ABS-G20 General Purpose PC/ABS Alloy, 20% Glass Filled
LG Chemical LUPOY GN5201F PC/ABS+GF20%, Halogen Free Flame Retardant
Covestro Bayblend® FR 3030 Polycarbonate + ABS, Flame Retardant Grade

PQZWA2428 / 91142

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.