MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Seals Eastern 5404 Nitrile Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: General purpose Nitrile

Information provided by Seals Eastern, Inc.

Key Words: NBR
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A >= 80>= 80ASTM D2240, Type A
 9090AVG; ASTM D2240, Type A
Tensile Strength at Break >= 12.59 MPa>= 1826 psiASTM D412 Method A
 19.09 MPa2769 psiAVG; ASTM D412 Method A
Tensile Stress at Strain  >= 2.68 MPa
@Strain 50 %
>= 389 psi
@Strain 50 %
Minimum; ASTM D412 Method A
 2.70 MPa
@Strain 25 %
391 psi
@Strain 25 %
Average; ASTM D412 Method A
 >= 4.57 MPa
@Strain 100 %
>= 663 psi
@Strain 100 %
Minimum; ASTM D412 Method A
 4.59 MPa
@Strain 50 %
666 psi
@Strain 50 %
Average; ASTM D412 Method A
 10.34 MPa
@Strain 100 %
1499 psi
@Strain 100 %
Average; ASTM D412 Method A
Elongation at Break >= 129 %>= 129 %ASTM D412 Method A
 182 %182 %AVG; ASTM D412 Method A
Modulus of Elasticity 0.02031 GPa2.946 ksiASTM D412 Method A
Poissons Ratio 0.500.50Calculated
Shear Modulus 0.00677 GPa0.982 ksiASTM D412 Method A
Secant Modulus 0.01909 GPa2.769 ksiASTM D412 Method A
 
Thermal PropertiesMetricEnglishComments
Glass Transition Temp, Tg -29.4 °C-21.0 °FASTM D1329
 
Descriptive Properties
Strain Energy / Unit Volume at 20% Elongation (psi)42

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Seals Eastern 5400 Nitrile Rubber
Seals Eastern 5401 Nitrile Rubber
Seals Eastern 7202 Nitrile Rubber
Seals Eastern 5353 Nitrile Rubber
Seals Eastern 7168 Nitrile Rubber

PSEAL10 / 80157

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.