MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Polygon Composites Polylube® HT High Temperature Bearings Versatile high load, low friction composite bearings
Categories: Polymer

Material Notes: PolyLube®HT bearing is a high load, low RPM bearing designed for applications where self-lubrication is desired, but conventional composite bearings will not perform high temperatures. This product has been designed to provide excellent performance at elevated temperatures. With a glass transition temperature of over 500°F this epoxy filament wound structure exhibits superb performance over extended exposure to elevated temperatures. The bearing material is focused on applications where the bearing will be exposed to temperatures up to 500°F. In addition to its high compressive properties (in both static and dynamic modes), this bearing material is inherently self-lubricating. The self-lubrication capability of Polygon’s new material means that the use of expensive high temperature external lubricants such as polyurea grease, lithium grease, some bentone greases, as well as advanced ester based oils and complex thickening systems may no longer be necessary. The PolyLube HT bearing creates a high strength, self-lubricating journal bearing material that can offer performance enhancements over greased systems, as well as graphite loaded bronze structures, some iron-copper graphites, polysulfone, PEEK, and polymide bearing materials.

Applications: PolyLube® High Temperature applications are not just for elevated temperature environments but also for applications where the bearing may need to resist thermal expansion during operation. One example of this is in snowmobile clutch markets. In these applications, the clutch speed goes from 0 to very high RPM’s in micro-seconds (and vice versa). During this cycling, friction is rising because speed is being dramatically increased. As the friction goes up so does the temperature of the associated components. A high temperature composite bearing material can resist these expansion phenomena and as a result offer better long term wear, improved bearing durability, and less seizure opportunity than conventional metal bearing materials.

Information provided by Polygon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.87 g/cc1.87 g/cc
Water Absorption  0.12 %
@Time 7200 sec
0.12 %
@Time 2.00 hour
 0.16 %
@Time 86400 sec
0.16 %
@Time 24.0 hour
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 138 MPa20000 psi
 827 MPa120000 psiHoop
Modulus of Elasticity 4.14 GPa600 ksi
 34.5 GPa5000 ksiTransverse
Flexural Strength 138 MPa20000 psi
Compressive Strength 483 MPa70000 psiUltimate, Radial
Poissons Ratio 0.0800.080Axial
Shear Modulus 4.14 GPa600 ksi
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.41e+15 ohm-cm2.41e+15 ohm-cm
Surface Resistance 2.92e+15 ohm2.92e+15 ohm
Insulation Resistance 2.38e+12 ohm
@Thickness 203 mm
2.38e+12 ohm
@Thickness 8.00 in
Dielectric Constant 4.15
@Frequency 60 Hz
4.15
@Frequency 60 Hz
Dielectric Strength 15.7 kV/mm400 kV/in
Dissipation Factor 0.0094
@Frequency 60 Hz
0.0094
@Frequency 60 Hz
 
Thermal PropertiesMetricEnglishComments
CTE, linear 8.64 µm/m-°C4.80 µin/in-°F
Specific Heat Capacity 1.13 J/g-°C0.270 BTU/lb-°F
Thermal Conductivity 0.259 - 0.331 W/m-K1.80 - 2.30 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 260 °C500 °F
Minimum Service Temperature, Air -212 °C-350 °F
 
Descriptive Properties
Heat Resistance500°FContinuous
Impulse400-550 V/mil11/2 40u Wave (Axial)
Maximum Velocity10 sfm
Power Factor10@ 60 cps (100v pct mx) – at 212°F
 10@ 60 cps (100v pct mx) – after 24 hrs at 100°F at 98% RH
 5@ 60 cps (100v pct mx) – as received
Unit Load Limit30000 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Parker Chomerics CHO-THERM® 1677 Thermally Conductive Insulator
Mueller Dynalloy Alloy 6730 Free cutting bearing bronze (UNS C67300)
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy)
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Cotronics Resbond™ 920 High Temperature Ceramic Adhesive, Thermally Conductive

PPOLYG08 / 184507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.