MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

AISI 1144 Steel, oil quenched 845°C (1550°F), 650°C (1200°F) temper, 100 mm (4 in.) round
Categories: Metal; Ferrous Metal; Carbon Steel; AISI 1000 Series Steel; Medium Carbon Steel

Material Notes: Applications include cold drawn or finished bar, cold punched nuts, split rivets, machine screws, and wood screws. Post oil quenched hardness: 27 HRC surface, 98 HRB half-radius, 97 HRB center.

Key Words: UNS G11440, ASTM A29, ASTM A108, ASTM A311, FED QQ-S-637 (C1144), SAE J403, SAE J412, SAE J414
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.87 g/cc0.284 lb/in³Typical for steel.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 183183
Hardness, Knoop 204204Converted from Brinell
Hardness, Rockwell B 8989Converted from Brinell
Hardness, Vickers 192192Converted from Brinell
Tensile Strength, Ultimate 615 MPa89200 psi
Tensile Strength, Yield 370 MPa53700 psi
Elongation at Break 25.8 %25.8 %
Reduction of Area 57.7 %57.7 %
Modulus of Elasticity 200 GPa29000 ksiTypical for steel
Bulk Modulus 160 GPa23200 ksiTypical for steel.
Poissons Ratio 0.290.29Typical For Steel
Shear Modulus 80.0 GPa11600 ksiTypical for steel.
Izod Impact 43.0 J31.7 ft-lbnormalized at 900°C (1650°F)
 53.0 J39.1 ft-lbas rolled
 65.0 J47.9 ft-lbannealed at 815°C (1500°F)
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000170 ohm-cm
@Temperature 20.0 °C
0.0000170 ohm-cm
@Temperature 68.0 °F
condition of specimen unknown
 
Thermal PropertiesMetricEnglishComments
CTE, linear  11.5 µm/m-°C
@Temperature 20.0 °C
6.39 µin/in-°F
@Temperature 68.0 °F
Typical steel
 12.2 µm/m-°C
@Temperature 0.000 - 300 °C
6.78 µin/in-°F
@Temperature 32.0 - 572 °F
Typical for steel
 13.9 µm/m-°C
@Temperature 0.000 - 500 °C
7.72 µin/in-°F
@Temperature 32.0 - 932 °F
Typical for steel
Specific Heat Capacity 0.472 J/g-°C0.113 BTU/lb-°FTypical steel
Thermal Conductivity 51.9 W/m-K360 BTU-in/hr-ft²-°FTypical steel
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.40 - 0.48 %0.40 - 0.48 %
Iron, Fe 97.5 - 98.01 %97.5 - 98.01 %As remainder
Manganese, Mn 1.35 - 1.65 %1.35 - 1.65 %
Phosphorus, P <= 0.040 %<= 0.040 %
Sulfur, S 0.24 - 0.33 %0.24 - 0.33 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
AISI 1144 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 13 mm (0.5 in.) round
AISI 1144 Steel, annealed at 790°C (1450°F), furnace cooled 11°C (20°F) per hour to 620°C, air cooled, 25 mm (1 in.) round
AISI 1144 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 25 mm (1 in.) round
AISI 1144 Steel, oil quenched 845°C (1550°F), 540°C (1000°F) temper, 50 mm (2 in.) round
AISI 1144 Steel, normalized at 900°C (1650°F), air cooled, 13 mm (0.5 in.) round

M114CS / 7285

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.