MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior Stanyl® TW200F8 PA46-GF40, Dry, 40% Glass Filled, Heat Stabilized
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 46 (PA46); Nylon 46, Glass Fiber Reinforced

Material Notes: 40% Glass Reinforced, Heat Stabilized

Former DSM Engineering Plastics product line is now with Envalior.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.51 g/cc0.0546 lb/in³ISO 1183
Moisture Absorption 2.20 %2.20 %Humidity; Sim. ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm0.0050 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm0.011 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 230 MPa33400 psiISO 527-1/-2
 100 MPa
@Temperature 200 °C
14500 psi
@Temperature 392 °F
ISO 527-1/-2
 105 MPa
@Temperature 180 °C
15200 psi
@Temperature 356 °F
ISO 527-1/-2
 115 MPa
@Temperature 160 °C
16700 psi
@Temperature 320 °F
ISO 527-1/-2
 130 MPa
@Temperature 120 °C
18900 psi
@Temperature 248 °F
ISO 527-1/-2
Elongation at Break 3.0 %3.0 %ISO 527-1/-2
 6.5 %
@Temperature 120 °C
6.5 %
@Temperature 248 °F
ISO 527-1/-2
 6.5 %
@Temperature 160 °C
6.5 %
@Temperature 320 °F
ISO 527-1/-2
 6.5 %
@Temperature 180 °C
6.5 %
@Temperature 356 °F
ISO 527-1/-2
 6.5 %
@Temperature 200 °C
6.5 %
@Temperature 392 °F
ISO 527-1/-2
Tensile Modulus 13.0 GPa1890 ksiISO 527-1/-2
 5.30 GPa
@Temperature 200 °C
769 ksi
@Temperature 392 °F
ISO 527-1/-2
 5.70 GPa
@Temperature 180 °C
827 ksi
@Temperature 356 °F
ISO 527-1/-2
 6.10 GPa
@Temperature 160 °C
885 ksi
@Temperature 320 °F
ISO 527-1/-2
 6.90 GPa
@Temperature 120 °C
1000 ksi
@Temperature 248 °F
ISO 527-1/-2
Flexural Modulus 11.5 GPa1670 ksiISO 178
 5.20 GPa
@Temperature 160 °C
754 ksi
@Temperature 320 °F
ISO 178
 5.80 GPa
@Temperature 120 °C
841 ksi
@Temperature 248 °F
ISO 178
Izod Impact, Notched (ISO)  12.0 kJ/m²
@Temperature -40.0 °C
5.71 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Charpy Impact Unnotched  7.50 J/cm²
@Temperature -30.0 °C
35.7 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 9.50 J/cm²
@Temperature 23.0 °C
45.2 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.20 J/cm²
@Temperature -30.0 °C
5.71 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+12 ohm-cm1.00e+12 ohm-cmIEC 60093
Dielectric Strength 30.0 kV/mm762 kV/inIEC 60243-1
Comparative Tracking Index 300 V300 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 25.0 µm/m-°C13.9 µin/in-°FISO 11359-1/-2
CTE, linear, Transverse to Flow 50.0 µm/m-°C27.8 µin/in-°FISO 11359-1/-2
Melting Point 295 °C563 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 290 °C554 °FISO 72-1/-2
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
IEC 60695-11-10
 HB
@Thickness 0.900 mm
HB
@Thickness 0.0354 in
IEC 60695-11-10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior Stanyl® TE263F6 PA46-I-GF30, Dry, 30% Glass Filled, Heat Stabilized, Impact Modified
Envalior Stanyl® SC50 PA46-GF30 FR, Conditioned, 30% Glass Filled, Flame Retardant
Envalior Stanyl® 46HF4550 PA46-GF50, Dry, 50% Glass Filled, Heat Stabilized
Envalior Stanyl® TE250F3 PA46-GF15 FR(15), Conditioned, 15% Glass Filled, Heat Stabilized, Flame Retardant
Envalior Stanyl® TS250F6D PA46-GF30 FR, Conditioned, 30% Glass Filled, Flame Retardant, Heat Stabilized

PDSM8237 / 184938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.