MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Avient Synprene® RT-3620 Thermoplastic Elastomer - SBC  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Styrenic TPE

Material Notes:

Description/Features:

  • Multi-Purpose Thermoplastic Elastomer
  • Natural

Applications:

  • General Purpose
  • Interior

Market:

  • Consumer Goods
  • Industrial

Processing Method:

  • Injection Molding
PolyOne First Choice

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.00 g/cc1.00 g/ccASTM D792
Linear Mold Shrinkage 0.010 cm/cm0.010 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2020Instant; ASTM D2240
Tensile Strength at Break 2.55 MPa370 psiMethod A (Dumbbell & Section), 20 in/min; ASTM D412
Tensile Stress at Strain 0.931 MPa
@Strain 300 %
135 psi
@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 730 %730 %Method A (Dumbbell & Section), 20 in/min; ASTM D412
Tear Strength 10.5 kN/m60.0 pliDie C (graves), 20 in/min; ASTM D624
Compression Set 12 %
@Temperature 23.0 °C,
Time 79200 sec
12 %
@Temperature 73.4 °F,
Time 22.0 hour
Method B; ASTM D395

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Santoprene® 8211-25 Thermoplastic Elastomer
Wacker Elastosil® LR 3003/20 TR A/B Liquid Silicone Rubber
Avient OnFlex™ S FR 25A-3S1830 Thermoplastic Elastomer (TPE)

PH1PO3232 / 44958

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.