MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil LD 302.32 High Clarity, High Impact Film Resin  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate Copolymer (EVA), Film Grade

Material Notes: LD 302 Series films exhibit superior impact strength, good heat sealability, and good low temperature properties. Typical applications are frozen food packaging or other food packaging.

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.923 g/cc0.0333 lb/in³ExxonMobil Method
Vinyl Acetate Content 3.5 %3.5 %ExxonMobil Method
Thickness 38.1 microns1.50 mil
Melt Flow 1.3 g/10 min1.3 g/10 minExxonMobil Method
Antiblock Level 2500 ppm2500 ppm
Slip Level 500 ppm500 ppm
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 8.27 MPa1200 psiat 2% offset; ASTM D882
Film Tensile Strength at Yield, TD 8.14 MPa1180 psiat 2% offset; ASTM D882
Film Elongation at Break, MD 190 %190 %ASTM D882
Film Elongation at Break, TD 580 %580 %ASTM D882
Film Elongation at Yield, MD 6.7 %6.7 %ASTM D882
Film Elongation at Yield, TD 5.7 %5.7 %ASTM D882
Elmendorf Tear Strength MD 190 g190 gASTM D1922
Elmendorf Tear Strength TD 110 g110 gASTM D1922
Elmendorf Tear Strength, MD 4.984 g/micron126.6 g/milASTM D1922
Elmendorf Tear Strength, TD 2.89 g/micron73.3 g/milASTM D1922
Dart Drop 4.461 g/micron113.3 g/milASTM D1709
Dart Drop Test 170 g0.375 lbASTM D1709
Film Tensile Strength at Break, MD 24.2 MPa3510 psiASTM D882
Film Tensile Strength at Break, TD 23.2 MPa3370 psiASTM D882
1% Secant Modulus, MD 146 MPa21200 psiASTM D882
1% Secant Modulus, TD 172 MPa24900 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 105 °C221 °FPeak Melting Temperature; ExxonMobil Method
Crystallization Temperature 92.0 °C198 °FExxonMobil Method
Vicat Softening Point 88.3 °C191 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 6.5 %6.5 %ASTM D1003
Gloss 69 %69 %45°; ASTM D2457
Transmission, Visible 90 %90 %clear; thickness not quantified
 
Descriptive Properties
FeaturesThermal Stabilizer

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LD 141.87 Shrink Film Resin
ExxonMobil LD 302.20 High Clarity, High Impact Film Resin
Eurofoam Evacell XM 2001 EVA + PE Foam
Eurofoam Evacell EVA 50/S EVA + NR Foam
Versalis Greenflex® FD 20 Ethylene Vinyl Acetate Copolymer - Blown Film Extrusion

PEXB003 / 37308

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.