MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sharadaa Ceramics ZAP 002 Smart Cast Application
Categories: Ceramic

Material Notes: Special Properties: Thermal Shock Slag Resistance

Industry: Steel

Application: Pig Iron Laddle working Layer

Information provided by Sharadaa Ceramics Pvt. Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density >= 2.65 g/cc>= 0.0957 lb/in³After Drying at 110°C
Grain Size <= 10000 µm<= 10000 µm
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength  39.2 MPa
@Temperature 110 °C
5690 psi
@Temperature 230 °F
Cold Crushing
 78.5 MPa
@Temperature 1100 °C
11400 psi
@Temperature 2010 °F
Cold Crushing
 98.1 MPa
@Temperature 1500 °C
14200 psi
@Temperature 2730 °F
Cold Crushing
 17.2 MPa
@Time 86400 sec
2490 psi
@Time 24.0 hour
Cold Crushing
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 1600 °C2910 °F
 
Descriptive Properties
Refractoriness>1720°C
Thermal Expansion0.65Reversible
Water Required to Mix9-11%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 1100-O
Solvay Chemicals Soda Solvay® Dense Soda Ash
Sharadaa Ceramics ZAP 008 Smart Cast Application
Overview of materials for Malleable Iron
Overview of materials for Gray Cast Iron

CSHARA126 / 130289

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.