MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Bicor® 85 AXT OPP Film  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: Product Description: Bicor ASB-X is a two side coated, sealable OPP film delivering an advanced level of moisture and oxygen battier protection. This film is designed for use in (unsupported and surface printed) horizontal or vertical packaging applications. It is also used as an outer web of laminations for vertical gas-flush applications.

Availability: Latin America, North America and South America

Key Features:

  • Robust machinability
  • Low and consistent COF
  • Excellent barrier performance
  • Outstanding flavor and aroma barrier
  • Excellent moisture barrier
  • Excellent oxygen barrier
Features:
  • Acrylic Coated
  • Flavor & Aroma Barrier
  • Gas Barrier
  • High Barrier Printable PVdC Coated
  • High Barrier PVdC Coated
  • In Lamination Lap Sealable
  • Moisture Barrier
  • Oxygen Barrier
  • PVdC Coated
  • Sealable High Barrier PVdC Coated
Applications:
  • Bakery
  • Biscuits/Cookie/Crackers
  • Box Overwrap
  • Confectionery, Gum
  • Confectionery, Sugar
  • Pet Food
Uses:
  • Box Overwrap Flexible Packaging
  • HFFS Flexible Packaging
  • Pre-made Bags - Flexible Packaging
  • VFFS Flexible Packaging
Processing Method: Cold Seal Adhesive, Inner Web Adhesive Lamination, Outer Web Adhesive Lamination, Outer Web Extrusion Lamination, Solvent Flexographic Printing, Solvent Rotogravure Printing, Surface Print Unsupported and Water-based Flexographic Printing

Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Water Vapor Transmission 3.10 g/m²/day
@Temperature 38.0 °C
0.200 g/100 in²/day
@Temperature 100 °F
90% RH; ExxonMobil Method
Oxygen Transmission Rate 6.20 cc/m²/day0.399 cc/100 in²/day23°C, 0% RH; ExxonMobil Method
Thickness 20.8 microns0.820 milNominal; ExxonMobil Method
Coating Weight 19.7 g/m²12.3 lb/reamExxonMobil Method
 
Mechanical PropertiesMetricEnglishComments
Coefficient of Friction 0.290.29Acrylic/Acrylic; ExxonMobil Method
Film Tensile Strength at Break, MD 117 MPa17000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
Film Tensile Strength at Break, TD 207 MPa30000 psi20 in/min, 2.0 in Jaw Separation; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Shrinkage, MD 4.5 %
@Temperature 135 °C
4.5 %
@Temperature 275 °F
ExxonMobil Method
Shrinkage, TD 3.0 %
@Temperature 135 °C
3.0 %
@Temperature 275 °F
ExxonMobil Method
 
Optical PropertiesMetricEnglishComments
Haze 1.5 %1.5 %ExxonMobil Method
Gloss 103 %103 %45º; ExxonMobil Method
 
Descriptive Properties
Crimp Seal MST 207°FPVdC/PVdC, 200g/in
Crimp Seal Strength600 g/inPVdC/PVdC, 260°F, 20psi, 3/4sec
Yield35000 in2/lb

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Bicor® 84 AOH OPP Film

PEXB382 / 37687

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.